Effects of Composition, Processing, and Structure on Properties of Composites
-
Published:1997
Abstract
This article describes the interaction of composition, manufacturing process, and composite properties of composites. The manufacturing process includes resin-matrix, metal-matrix, and carbon/carbon matrix processing. The article discusses various mechanical properties of composites. It explores how variations in the composition, manufacturing, shop process instructions, and loading/environmental conditions can affect the use of a composite product in a performance/service life operation.
Sign in
ASM members
Member Sign InR. Laramee, Effects of Composition, Processing, and Structure on Properties of Composites, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 457–469, https://doi.org/10.31399/asm.hb.v20.a0002465
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.