Design for Powder Metallurgy[1]
-
Published:1997
Abstract
This article begins with a discussion on general powder metallurgy design considerations that assist in the selection of the appropriate processing method. It reviews powder processing techniques, conventional press-and-sinter methods, and full-density processes to understand the design restrictions of each powder processing method. The article provides comparison of powder processing methods based on their similarities, differences, advantages, and disadvantages. It concludes with a discussion on design issues for the components of powder processing technologies.
Sign in
ASM members
Member Sign InHoward I. Sanderow, Design for Powder Metallurgy, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 745–753, https://doi.org/10.31399/asm.hb.v20.a0002486
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.