Modeling and Simulation of Metal Powder Injection Molding Available to Purchase
-
Published:2010
Abstract
This article focuses on the axisymmetric 2.5-dimensional approach used in metal powder injection molding (PIM) simulations. It describes three stages of PIM simulations: filling, packing, and cooling. The article discusses the process features of numerical simulation of PIM, such as filling and packing analysis, cooling analysis, and coupled analysis between filling, packing, and cooling stages. It explains the experimental material properties and verification for filling, packing, and cooling stages in the PIM simulations. The article presents simulation results from some of the 2.5-dimensional examples to demonstrate the usefulness of the computer-aided engineering analysis and optimization capability of the PIM process.
Seokyoung Ahn, Seong-Taek Chung, Seong Jin Park, Randall M. German, Modeling and Simulation of Metal Powder Injection Molding, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 343–357, https://doi.org/10.31399/asm.hb.v22b.a0005503
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.