Simulation of Induction Heat Treating
-
Published:2010
Abstract
This article describes the applications of induction heat treatment of metals, including normalizing, annealing, hardening, and tempering and stress relieving. It discusses the simulation techniques of the electromagnetic and thermal processes that occur during induction heat treating. The article explains the finite-difference method, finite-element method, mutual impedance method, and boundary-element method for the numerical computation of the induction heat treating processes. It also discusses the direct and indirect coupling approaches for coupling the electromagnetic and heat-transfer problems. Modern computer simulation techniques are capable of effectively simulating electromagnetic and thermal phenomena for many processes that involve electromagnetic induction. The article considers the challenges faced by developers of modern simulation software.
Valery Rudnev, Simulation of Induction Heat Treating, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 501–546, https://doi.org/10.31399/asm.hb.v22b.a0005533
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.