Modeling of Porosity Formation during Solidification
-
Published:2010
Abstract
There is a need for models that predict the percentage and size of porosity formed during solidification in order to effectively predict mechanical properties. This article provides an overview of equations that govern pore formation. It reviews the four classes of models, highlighting both the benefits and drawbacks of each class. These classes include criteria functions, analytical models, continuum models, and kinetic models. The article also tabulates the criteria functions for porosity prediction.
Sign in
ASM members
Member Sign InPeter D. Lee, Junsheng Wang, Modeling of Porosity Formation during Solidification, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 253–263, https://doi.org/10.31399/asm.hb.v22b.a0005520
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.