Metals Process Simulation
Formation of Microstructures, Grain Textures, and Defects during Solidification
-
Published:2010
Abstract
This article reviews the various aspects of the simulation of solidification microstructures and grain textures. It describes the grain structures and morphology of dendrites or eutectics that compose the internal structure of the grains. A particular emphasis has been put on the simulation of defects related to grain textures and microstructures. The article provides information on the application of the most important simulation approaches and the status of numerical simulation.
A. Jacot, Ch.-A. Gandin, Formation of Microstructures, Grain Textures, and Defects during Solidification, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 214–227, https://doi.org/10.31399/asm.hb.v22b.a0005518
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.