Metals Process Simulation
Thermophysical Properties
-
Published:2010
Abstract
This article presents typical values for the most used types of thermophysical property data that are needed for processing and modeling of solidification and casting processes. It describes methods to determine thermophysical properties, such as specific heat capacity and enthalpy of transformation; enthalpy of melting; solidus and liquidus temperatures; coefficient of thermal expansion; density; surface tension; viscosity; electrical and thermal conductivity; and emissivity.
Sign in
ASM members
Member Sign InJuan J. Valencia, Peter N. Quested, Thermophysical Properties, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 18–32, https://doi.org/10.31399/asm.hb.v22b.a0005523
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.