Computational Analysis of the Vacuum Arc Remelting (VAR) and Electroslag Remelting (ESR) Processes
-
Published:2010
Abstract
This article provides an overview of the studies on computational modeling of the vacuum arc remelting (VAR) and electroslag remelting (ESR) processes. These models involve the axisymmetric analysis of the electromagnetic, flow, heat-transfer, and phase-change phenomena to predict the pool shape and thermal history of an ingot using two-dimensional axisymmetric models for VAR and ESR. Analysis of segregation of alloying elements during solidification that gives rise to macrolevel compositional nonuniformity in titanium alloy ingots is also described. The article discusses the important features of the control-volume-based computational method to review the unique aspects of the processes. Measurement of the...
Sign in
ASM members
Member Sign InKanchan M. Kelkar, Suhas V. Patankar, Alec Mitchell, Ramesh S. Minisandram, Ashish D. Patel, Computational Analysis of the Vacuum Arc Remelting (VAR) and Electroslag Remelting (ESR) Processes, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 196–213, https://doi.org/10.31399/asm.hb.v22b.a0005510
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!