Abstract
This article discusses the three different modeling approaches for grain structures formed during solidification of metallic alloys: direct modeling of dendritic structure, direct modeling of grain structure, and indirect modeling of grain structure. The main construction bases, the scale at which it applies, and the mathematical background are presented for each modeling approach. The article concludes with a table that presents a comparison of the main inputs/outputs, approximations, numerical methods, kinetics laws, and applications for the three approaches to modeling of dendritic grain solidification.
Sign in
ASM members
Member Sign InCh.-A. Gandin, A. Jacot, Modeling of Dendritic Grain Solidification, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 228–239, https://doi.org/10.31399/asm.hb.v22b.a0005521
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!