Metals Process Simulation
Simulation of Powder Metallurgy Processes
-
Published:2010
Abstract
Power metallurgy (PM) is a process of shaping metal powders into near-net or net shape parts combined with densification or consolidation processes for the development of final material and design properties. This article introduces the general considerations, models, and applications in the modeling of PM processes. It describes the PM process in terms of powder compaction and sintering. The article schematically illustrates powder injection molding for the production of plastic parts and describes PM process models such as discrete-element model (DEM), linear continuum model, and nonlinear continuum model. It concludes with information on the application of press and sinter...
Sign in
ASM members
Member Sign InSimulation of Powder Metallurgy Processes, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.