Abstract
This article discusses physical analysis, including slab method and upper-bound method and slip-line field analysis, for calculating stress states in plastic deformation processes. It presents various validation standards and models for evaluating the criterion of fracture for use in finite-element analyses of deformation processing. The article reviews the Cockcroft-Latham criterion of fracture and its reformulated extension for analysing the fracture locus for compression. It concludes with information on fundamental fracture models.
Howard Kuhn, Models for Fracture during Deformation Processing, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 346–361, https://doi.org/10.31399/asm.hb.v22a.a0005461
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.