This article describes the models of physical phenomena involving solution of differential equations such as ordinary or partial differential equations. It reviews the basic concepts of differential calculus and tabulates the expansion of functions into power series. A table of linear partial differential equations is also presented.
Topics
Modeling tools and methods
You do not currently have access to this chapter.
Citation
Differential Calculus and Equations, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 673–682, https://doi.org/10.31399/asm.hb.v22a.a0005453
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Electromagnetic Problem Solutions
Induction Heating and Heat Treatment