Abstract
Neural networks permit the discovery of fundamental relationships and quantitative structure within vast arrays of ill-understood data. This article provides an overview of neural network modeling method, describing its overfitting nature. It discusses the use of neural networks in modeling noise and uncertainties in conducting experiments. The article also presents examples of the application of neural-network modeling to the behavior of metals.
H.K.D.H. Bhadeshia, H.J. Stone, Neural-Network Modeling, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 435–439, https://doi.org/10.31399/asm.hb.v22a.a0005416