Network and Vertex Models for Grain Growth Available to Purchase
-
Published:2009
Abstract
This article reviews network models and their applications for the simulation of various physical phenomena related to grain-boundary migration. It discusses the steps involved in the implementation of two and three-dimensional network models, namely, acquisition and discretization of the microstructure, formulation of the equation of motion, and implementation of the topological transformations. The article presents examples that illustrate the simulation of physical phenomena to demonstrate the predictive power and flexibility of network models.
L.A. Barrales Mora, V. Mohles, G. Gottstein, L.S. Shvindlerman, Network and Vertex Models for Grain Growth, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 282–296, https://doi.org/10.31399/asm.hb.v22a.a0005422
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.