Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys Available to Purchase
-
Published:2009
Abstract
This article summarizes the general features of microstructure evolution during the thermomechanical processing (TMP) of nickel-base superalloys and the challenges posed by the modeling of such phenomena. It describes the fundamentals and implementations of various modeling methodologies. These include JMAK (Avrami) models, topological models, and mesoscale physics-based models.
J.P. Thomas, F. Montheillet, S. L. Semiatin, Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 566–582, https://doi.org/10.31399/asm.hb.v22a.a0005459
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.