Abstract
This article presents a diagramatic representation of a periodic system that illustrates the fundamental alloying nature of iron for ferrous metallurgists.
Topics
Iron
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Periodic System for Ferrous Metallurgists, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 587, https://doi.org/10.31399/asm.hb.v22a.a0005440
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Principles of Alloying
Alloying Understanding the Basics
Glossary of Terms: Surface Engineering
Surface Engineering
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Low-Expansion Alloys
Alloying Understanding the Basics
Magnetic Alloys
Alloying Understanding the Basics
Introduction to Steels and Cast Irons
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels
Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Fatigue Fracture of Waspaloy Spray-Manifold Assembly Because of Embrittlement by Penetration of Molten Braze Metal
ASM Failure Analysis Case Histories: Processing Errors and Defects
Introduction to Corrosion Resistance of Bulk Materials
Corrosion: Fundamentals, Testing, and Protection