Abstract
This article is a comprehensive collection of fluid dynamic equations for properties of fluids, fluid statics, fluid motion, dimensional analysis, and boundary layer flow. It presents equations for analyzing problems in fluid mechanics, continuity equation, momentum equation, and energy equation for solving various problems related to fluid dynamics.
You do not currently have access to this chapter.
Citation
Fluid Dynamic Equations, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 659–672, https://doi.org/10.31399/asm.hb.v22a.a0005450
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Modeling of Heat and Mass Transfer in Fusion Welding
Welding Fundamentals and Processes
Numerical Aspects of Modeling Welds
Welding, Brazing, and Soldering
Useful Formulas for Metals Processing
Metals Process Simulation