Simulation of Microstructural Evolution in Steels
-
Published:2009
Abstract
Computer simulation of microstructural evolution during hot rolling of steels is a major topic of research and development in academia and industry. This article describes the methodology and procedures commonly employed to develop microstructural evolution models to simulate microstructural evolution in steels. It presents an example of the integration of finite element modeling and microstructural evolution models for the simulation of metal flow and microstructural evolution in a hot rolling process.
P.M. Pauskar, R. Shivpuri, Simulation of Microstructural Evolution in Steels, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 491–509, https://doi.org/10.31399/asm.hb.v22a.a0005414