Constitutive Models for Superplastic Flow Available to Purchase
-
Published:2009
Abstract
This article presents a mechanical description of superplasticity and discusses constitutive equations that are essential for simulating superplastic forming processes, applicable to structural superplasticity. It presents the phenomenological constitutive equations of superplasticity and classical physical constitutive equations. The article also reviews the accommodation mechanisms that are divided into two major groups, namely, diffusional accommodation and accommodation by dislocations.
Indrajit Charit, Rajiv S. Mishra, Constitutive Models for Superplastic Flow, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 472–477, https://doi.org/10.31399/asm.hb.v22a.a0005433
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.