Modeling of Deformation Processes—Slab and Upper Bound Methods Available to Purchase
By
Rajiv Shivpuri
Rajiv Shivpuri
The Ohio State University
Search for other works by this author on:
-
Published:2009
Page range:
23 - 33
Abstract
This article focuses on approximate closed-form analytical methods, such as slab and upper bound methods, used for forward and inverse design of metal forming problems. Selected examples of application of these methods to metal forming processes are also discussed.
You do not currently have access to this chapter.
Citation
Rajiv Shivpuri, Modeling of Deformation Processes—Slab and Upper Bound Methods, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 23–33, https://doi.org/10.31399/asm.hb.v22a.a0005456
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Springback
Metalworking: Sheet Forming
Deep Drawing of Round and Rectangular Cups
Sheet Metal Forming Fundamentals
Models for Fracture during Deformation Processing
Fundamentals of Modeling for Metals Processing
Methods of Analysis for Forging Operations
Cold and Hot Forging Fundamentals and Applications
Environmental and Application Factors in Solid Friction
Friction, Lubrication, and Wear Technology
Wire, Rod, and Tube Drawing
Metalworking: Bulk Forming
Measurement and Interpretation of Flow Stress Data for the Simulation of Metal-Forming Processes
Metals Process Simulation
An Investigation of the Development of Defects During Flow Forming of High Strength Thin Wall Steel Tubes
ASM Failure Analysis Case Histories: Processing Errors and Defects
Surfaces and Friction
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Fundamentals of Tribology in Metal Forming
Friction, Lubrication, and Wear Technology