Skip Nav Destination
ASM Handbook
Fundamentals of Modeling for Metals ProcessingAvailable to Purchase
Edited by
ASM International
Volume
22A
ISBN electronic:
978-1-62708-196-2
Publication date:
2009
Book Chapter
Vapor Pressures of the Elements Available to Purchase
-
Published:2009
Page range:
608
Abstract
This article contains a table that lists the vapor pressures of selected metallic elements.
You do not currently have access to this chapter.
Citation
Vapor Pressures of the Elements, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 608, https://doi.org/10.31399/asm.hb.v22a.a0005446
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Crystal Structures and Lattice Parameters of Allotropes of the Metallic Elements
Alloy Phase Diagrams
Crystal Structure of Metallic Elements
Metals Handbook Desk Edition (2nd Edition)
Vapor Phase Corrosion Inhibitors
Corrosion: Fundamentals, Testing, and Protection
Physical and Nuclear Properties
Beryllium Chemistry and Processing