Abstract
This article contains a table that lists the electrical conductivity and resistivity of selected metals, alloys, and materials at ambient temperature. These include aluminum and aluminum alloys; copper and copper alloys; electrical heating alloys; instrument and control alloys; relay steels and alloys; thermostat metals; electrical contact materials; and magnetically soft materials.
You do not currently have access to this chapter.
Citation
Electrical Conductivity of Metals and Alloys, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 606–607, https://doi.org/10.31399/asm.hb.v22a.a0005445
Download citation file:
Related Book Content
Corrosion of Nonferrous Alloy Weldments
Corrosion of Weldments
Coextrusion Welding
Welding, Brazing, and Soldering
Forge and Coextrusion Welding
Welding Fundamentals and Processes
Linear Thermal Expansion of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Heat Treatable Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Projection Welding
Welding Fundamentals and Processes
Biological Corrosion Failures
Failure Analysis and Prevention
Thermal Softening and Stress Relaxation in Copper
Metals Handbook Desk Edition (2nd Edition)
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Thermal Conductivity of Metals and Alloys
Fundamentals of Modeling for Metals Processing