Thermal Conductivity of Metals and Alloys
-
Published:2009
Page range:
604 - 605
Abstract
This article contains a table that lists the thermal conductivity of selected metals and alloys near room temperature. These include aluminum and aluminum alloys; copper and copper alloys; iron and iron alloys; lead and lead alloys; magnesium and magnesium alloys; nickel and nickel alloys; tin and tin alloys; titanium and titanium alloys; zinc and zinc alloys; and pure metals.
You do not currently have access to this chapter.
Citation
Thermal Conductivity of Metals and Alloys, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 604–605, https://doi.org/10.31399/asm.hb.v22a.a0005444
Download citation file:
Related Book Content
Linear Thermal Expansion of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Density of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Heat Treatable Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Metallography and Microstructures of Zinc and Its Alloys
Metallography and Microstructures
Density of Metals and Alloys
Corrosion: Materials
Corrosion of Metal Artifacts Displayed in Outdoor Environments
Corrosion: Environments and Industries
Heat Treatment of Nonferrous Alloys
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treatment of Aluminum and Other Nonferrous Alloys
Practical Heat Treating Basic Principles
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)