Fundamentals of Modeling for Metals Processing
Abstract
This article contains a table that lists the density of metals and alloys. It presents information on aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, and zinc, an their respective alloys. Information on wrought alloys, permanent magnet materials, precious metals, and rare earth metals is also listed.
Sign in
ASM members
Member Sign InDensity of Metals and Alloys, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 599–601, https://doi.org/10.31399/asm.hb.v22a.a0005442