Reference Information
-
Published:2012
Abstract
This article contains a table that lists the ISO standards for the biological evaluation of medical devices.
Abstract
This article tabulates materials that are known to have been used in orthopaedic and/or cardiovascular medical devices. The materials are grouped as metals, ceramics and glasses, and synthetic polymers in order. These tables were compiled from the Medical Materials Database which is a product of ASM International and Granta Design available by license online and as an in-house version. The material usage was gleaned from over 24,000 U.S. Food and Drug Administration (USFDA), Center for Devices and Radiological Health, Premarket notifications...
Sign in
ASM members
Member Sign InReference Information, Materials for Medical Devices, Vol 23, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2012
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.