Magnetic-particle inspection is a method of locating surface and subsurface discontinuities in ferromagnetic materials. This article discusses the applications and advantages and limitations of magnetic-particle inspection. It describes magnetic fields in terms of magnetized ring, magnetized bar, circular magnetization, longitudinal magnetization, and effects of flux direction. General applications, advantages, and limitations of the various magnetizing methods used in magnetic-particle inspection are listed in a table. The article discusses the items that must be considered in establishing a set of procedures for the magnetic-particle inspection of a specific part: type of current, type of magnetic particles, method of magnetization, direction...
Sign in
ASM members
Member Sign InDavid Eisenmann, Magnetic-Particle Inspection, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 96–123, https://doi.org/10.31399/asm.hb.v17.a0006468
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.