Ultrasonic Imaging and Sizing[1]
-
Published:2018
Abstract
This article discusses the inspection/reference standards that are absolutely critical for proper application of ultrasonic inspection systems. Many of the standards and specifications for ultrasonic inspection require the use of standard reference blocks. The article lists the variables that should be considered when selecting standard reference blocks and describes the three types of standard blocks ordinarily used for calibration or reference: area-amplitude blocks, distance-amplitude blocks, and blocks of the type sanctioned by the International Institute of Welding. It reviews the determination of area-amplitude and distance-amplitude curves of a straight-beam pulse-echo ultrasonic inspection system. The article discusses the three principal conventional manual ultrasonic sizing techniques: 6 dB drop technique, maximum-amplitude technique, and 20 dB drop technique. It provides information on the dimension-measurement applications of ultrasonic inspection methods.
Leonard J. Bond, Mica Baquera, Ultrasonic Imaging and Sizing, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 291–321, https://doi.org/10.31399/asm.hb.v17.a0006473
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.