Computed Tomography[1]
Revising author
Revising author
-
Published:2018
Abstract
Computed tomography (CT) is an imaging technique that generates a three-dimensional (3-D) volumetric image of a test piece. This article illustrates the basic principles of CT and provides information on the types, applications, and capabilities of CT systems. A comparison of performance characteristics for film radiography, real-time radiography, and X-ray computed tomography is presented in a table. A functional block diagram of a typical computed tomography system is provided. The article discusses CT scanning geometry that is used to acquire the necessary transmission data. It also provides information on digital radiography, image processing and analysis, dual-energy imaging, and partial...
Sign in
ASM members
Member Sign InAndrea Scanavini, Marco Moscatti, Computed Tomography, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 440–474, https://doi.org/10.31399/asm.hb.v17.a0006456
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!