Nondestructive Evaluation of Materials
Standards and Codes for Nondestructive Testing
-
Published:2018
Abstract
This article is a brief guide to information sources on nondestructive testing (NDT). It provides examples of some of the standards bodies commonly used by NDT personnel. These include the American Society for Testing and Materials (ASTM) International, European Committee for Standardization (CEN), American Society of Mechanical Engineers (ASME), International Organization for Standardization (ISO), Aerospace Industries Association (AIA), American Welding Society (AWS), American Petroleum Institute (API), and American Society for Nondestructive Testing (ASNT). All of these organizations used industry subject-matter experts and a consensus process in the development of their codes and standards.
Sign in
ASM members
Member Sign InStandards and Codes for Nondestructive Testing, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 661–662, https://doi.org/10.31399/asm.hb.v17.a0006479
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.