Nondestructive Evaluation of Materials
Thermoelastic Stress Analysis
-
Published:2018
Abstract
Thermoelastic stress analysis (TSA) an increasingly popular infrared (IR)-based technique for measuring stress on the surface of a part subjected to time-varying loads. This article begins by providing a theoretical and historical background of thermoelastic stress analysis. It then describes infrared detectors, such as quantum detectors and thermal/nonquantum detectors, for thermoelastic stress analysis. The article discusses the theoretical aspects for producing thermoelastic stress analysis data and the applications amenable to thermoelastic stress analysis. It concludes with information on the qualitative applications of thermoelastic stress analysis.
Sign in
ASM members
Member Sign InDavid Backman, Thermoelastic Stress Analysis, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 143–151, https://doi.org/10.31399/asm.hb.v17.a0006451
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.