Nondestructive Evaluation of Materials
Laser-Ultrasonics—Principles and Industrial Applications
-
Published:2018
Abstract
Laser-ultrasonics is a particular implementation of ultrasonic nondestructive inspection in which ultrasound is generated and detected by lasers. This article discusses the various mechanisms that ensure ultrasound generation and explains the possibility to get the equivalent of phase-array by numerical processing of an array of previously acquired laser-ultrasonic signals. The article describes the ultrasound generation by thermoelastic mechanism and ablation or vaporization. It illustrates the principle of optical detection of ultrasound with confocal Fabry-Perot interferometer and photorefractive two-wave mixing interferometer. The article concludes with information on the industrial applications of laser-ultrasonics, including thickness measurement, flaw detection, and material characterization....
Sign in
ASM members
Member Sign InJean-Pierre Monchalin, Laser-Ultrasonics—Principles and Industrial Applications, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 238–258, https://doi.org/10.31399/asm.hb.v17.a0006460
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.