Nondestructive Evaluation of Materials
Acoustic Microscopy[1]
Revising author
Revising author
-
Published:2018
Abstract
This article discusses the fundamentals and operating principles of the following acoustic microscopy methods: scanning laser acoustic microscopy, C-mode scanning acoustic microscopy, and scanning acoustic microscopy. It describes the applications of acoustic microscopy for detecting defects in metals, ceramics, glasses, polymers, and composites with examples.
Sign in
ASM members
Member Sign InBernhard R. Tittmann, Lawrence W. Kessler, Acoustic Microscopy, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 331–352, https://doi.org/10.31399/asm.hb.v17.a0006466