Digital Imaging–Real-Time, Computed, and Digital Radiography[1]
Revising author
-
Published:2018
Abstract
Digital radiography is a technique that uses digital detector arrays (linear or area) to capture an X-ray photonic signal and convert it to an electronic signal for display on a computer. This article begins with an overview of real-time radiography and provides a schematic illustration of a typical radioscopic system using an X-ray image intensifier. It discusses the advantages and limitations of real-time radiography. Computed radiography (CR) is one of the radiography techniques that utilizes a reusable detector comprised of photostimuable luminescence (PSL) storage phosphor. The article provides a schematic illustration of a typical storage phosphor imaging plate. It...
Sign in
ASM members
Member Sign InScott McClain, Claudia Kropas-Hughes, Digital Imaging–Real-Time, Computed, and Digital Radiography, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 436–439, https://doi.org/10.31399/asm.hb.v17.a0006459
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!