Magnetic Barkhausen Noise for Nondestructive Inspection of Gears
-
Published:2018
Abstract
Gears are a common part type for applications of the magnetic Barkhausen noise (MBN) techniques for nondestructive inspection. This article discusses the typical applications for MBN techniques, namely, detection of grinding retemper burn, evaluation of residual stresses, and detection of heat treatment defects, including the evaluation of case depth.
Sign in
ASM members
Member Sign InJames Thomas, Magnetic Barkhausen Noise for Nondestructive Inspection of Gears, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 590–593, https://doi.org/10.31399/asm.hb.v17.a0006476