Microwave- and Millimeter-Wave Inspection[1] Available to Purchase
-
Published:2018
Abstract
Electromagnetic signals at microwave and millimeter-wave frequencies are well suited for inspecting dielectric materials and composite structures in many critical applications. This article presents a partial list of reported nondestructive testing (NDT) application areas for microwaves. It discusses the advantages and limitations of inspection with microwaves. The article discusses the physical principles, including reflection and refraction, absorption and dispersion, scattering, and standing waves. It provides a discussion on terahertz (THz) imaging for nondestructive evaluation (NDE). The article concludes with information on ground-penetration radar (GPR) that uses electromagnetic radiation and detects the reflected signals from subsurface structures.
Microwave- and Millimeter-Wave Inspection, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 508–514, https://doi.org/10.31399/asm.hb.v17.a0006475
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.