Abstract
The main factors affecting the mechanical properties of compacted graphite irons both at room temperatures and at elevated temperatures are composition, structure (nodularity and matrix), and section size. This article presents a comparison between some properties of flake graphite (FG), compacted graphite (CG), and spheroidal graphite (SG) irons in a table. It discusses the effects of composition, structure, and section size on the mechanical properties of compacted graphite irons. The compressive and shear properties, modulus of elasticity, impact properties, fatigue strength, and elevated-temperature properties of compacted graphite irons are also reviewed.
Mechanical Properties of Compacted Graphite Iron, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 472–480, https://doi.org/10.31399/asm.hb.v01a.a0006346
Download citation file:
Data Ecosystem
The ASM Data Ecosystem arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.