From the point of view of economics and ecology, thin-wall ductile iron (TWDI) castings can compete in terms of mechanical properties with the light castings made of aluminum alloys. This article discusses the effect of technological factors on the cooling rate and physicochemical state of the liquid metal for preparing thin-wall castings with good mechanical properties and performance while avoiding casting defects. It describes a variety of defects that may appear during the production of TWDI castings, such as casting skin anomalies (e.g., flake graphite, graphite segregation), graphite clusters, exploded graphite, slag inclusions, shrinkage porosity, eutectic chill and secondary carbides, and cold shuts. The article reviews the tensile, fatigue, impact, and wear properties of TWDI castings. It provides information on the production and applications of TWDI castings.
Marcin Górny, Doru M. Stefanescu, Thin-Wall Ductile Iron Castings, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 617–628, https://doi.org/10.31399/asm.hb.v01a.a0006327
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.