Brazing and Soldering of Cast Irons
Reviewing author
-
Published:2017
Abstract
Brazing and soldering are done at temperatures below the solidus temperature of the base material but high enough to melt the filler metal and allow the liquid filler metal to wet the surface and spread into the joint gap by capillary action. This article discusses the common advantages of both brazing and soldering. It describes the brazing and soldering of cast irons, as well as the selection of brazing filler material. The article discusses various brazing methods: torch brazing, induction brazing, salt-bath brazing, and furnace brazing. It concludes with information on the application examples of brazing of cast iron....
Sign in
ASM members
Member Sign InCharles White, Brazing and Soldering of Cast Irons, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 310–318, https://doi.org/10.31399/asm.hb.v01a.a0006302
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!