This article focuses on friction, lubrication, and wear of internal combustion engine parts, improvements in which provide important gains in energy efficiency, performance, and longevity of the internal combustion (IC) engine systems. It discusses the types, component materials, and Friction and Wear Control of IC engine. The article explains the process of friction reduction by surface textures or coatings. It provides information on surface hardening of iron and steel, which is commonly employed for engine and powertrain components such as crankshafts, cams, and cylinder liners. The article also discusses advanced surface engineering technologies, such as diamondlike carbon coatings and...
Sign in
ASM members
Member Sign InVictor W. Wong, Simon C. Tung, Friction, Lubrication, and Wear of Internal Combustion Engine Parts, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 899–915, https://doi.org/10.31399/asm.hb.v18.a0006427
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!