Book Chapter
Environmental and Application Factors in Solid Friction
-
Published:2017
Abstract
This article focuses on environmental and application factors in solid friction. It covers the tribology of contact between a soft and hard material, including mechanisms and testing. The article describes the tribology of contact between a metal and tool during metalworking processes. It also discusses the tribology of metal friction at elevated temperatures.
You do not currently have access to this chapter.
Citation
Environmental and Application Factors in Solid Friction, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 81–101, https://doi.org/10.31399/asm.hb.v18.a0006410
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Preface
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Symbols
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Common Abbreviations
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
About the Author
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Background and Method of Treatment
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Conversion Factors and Definitions
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Springback
Metalworking: Sheet Forming
Tribology, Tribosystems, and Related Terminology
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Modeling of Deformation Processes—Slab and Upper Bound Methods
Fundamentals of Modeling for Metals Processing
Introduction to Tribology and Tribological Parameters
Friction, Lubrication, and Wear Technology