Tribocorrosion[1] Available to Purchase
Revising author
-
Published:2017
Abstract
Tribocorrosion is the subject dealing with complex, synergistic effects of chemical and mechanical conditions that cause wear. This article begins with a discussion on oxidative wear and corrosive wear, as well as quantitative measurements of corrosion, mechanical wear, and wear-corrosion effects. It illustrates the mechanism of corrosive-abrasive wear and discusses the factors affecting two-body wear. These factors include particle shape, size, density, and hardness; slurry velocity; slurry particle angle of attack; solids concentration in the slurry; hydrodynamic factors; corrosion products and the mass transfer of oxygen. The article describes slurry particle impingement tests and grinding tribocorrosion tests, as well as the factors to be considered for mitigating corrosive wear, such as materials selection, surface treatments, and environment modifications.
Andrew W. Batchelor, Tribocorrosion, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 351–361, https://doi.org/10.31399/asm.hb.v18.a0006415
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.