Friction, Lubrication, and Wear of Pump and Compressor Components
-
Published:2017
Abstract
Pumps and compressors are representative fluid machineries, which are indispensably important industrial equipment for water supply systems, chemical processing and reactions, and fluid power systems. This article addresses friction, lubrication, and wear of components in several types of machines such as positive displacement pumps including hydraulic pumps, turbo-pumps including centrifugal pumps, vacuum pumps, and compressors including the positive displacement type and turbo type.
Toshiharu Kazama, Friction, Lubrication, and Wear of Pump and Compressor Components, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 945–956, https://doi.org/10.31399/asm.hb.v18.a0006429