Frictional Heating in Dry and Lubricated Contacts
-
Published:2017
Abstract
This article provides an overview of experimental, analytical, and numerical tools for temperature evaluation of dry and lubricated systems. It describes the analytical methods and numerical techniques for frictional heating and temperature estimation, as well as viscous heating in full-film lubrication. The article also discusses the viscous heating temperature measurements and numerical analysis of viscous heating.
Jacob Sukumaran, Patrick De Baets, Dieter Fauconnier, Frictional Heating in Dry and Lubricated Contacts, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 67–80, https://doi.org/10.31399/asm.hb.v18.a0006409