Friction, Lubrication, and Wear Technology
Tribology of Power Train Systems
-
Published:2017
Abstract
Tribology is the study of friction, lubrication, and wear. It is a multidisciplinary subject covering the mechanics of contacting surfaces, their roughness characteristics, lubrication, and material behavior under normal load as well as in traction. This article focuses on well-established and widely accepted analytical methods and design and analysis charts for dealing with some of the issues in the area of engine and power train tribology. It provides a discussion on lubricant rheology and the prediction of lubricating film thickness. The article reviews the frictional power loss in piston-cylinder conjunctions, engine bearings, and transmission and differential gearing systems.
Sign in
ASM members
Member Sign InH. Rahnejat, R. Rahmani, M. Mohammadpour, P.M. Johns-Rahnejat, Tribology of Power Train Systems, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 916–934, https://doi.org/10.31399/asm.hb.v18.a0006399
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.