The human internal environment plays a vital role in the friction and wear of implants and prosthetic devices. This article describes the tribological/wear behavior of implants. It discusses the classification of active tribological pairs, namely, amphiarthosis joints and diarthosis joints. The article details the classification of total knee replacement, depending on the type of mechanical stability, including nonconstrained knee replacement, semiconstrained knee replacement, and constrained knee replacement. It also discusses the classifications of passive tribological pairs, namely, total disc replacement in the spine, dental implants, and temporomandibular joint. It describes the various testing methods for characterizing the implant materials used in hip, knee, spine, and dental applications. The article also describes the typical standards used for testing wear behavior of tribological pairs, namely, hip-wear simulation standards, knee-wear simulation standards, and spinal disc-wear simulation standards.
Andrew W. Batchelor, Margam Chandrasekaran, Biotribology of Medical Implants, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 372–378, https://doi.org/10.31399/asm.hb.v18.a0006404
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.