This article focuses on different aspects of wear particle analysis. It discusses the different wear regimes in the wear rate versus time (bathtub) curve. The article explains the essence of condition monitoring and how to properly sample lubricants for condition monitoring. It also discusses in-service lubricant analysis for condition monitoring, focusing on the spectrometric oil analysis program. The article describes the characteristics of wear particles and analytical techniques for characterizing them. It also describes the characteristics of different types of wear particles and the mechanisms by which they are generated. The article concludes with a summary of the major applications of wear particle analysis.
Noam Eliaz, Wear Particle Analysis, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 1010–1031, https://doi.org/10.31399/asm.hb.v18.a0006383
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.