Friction and Wear of Sliding Bearings Available to Purchase
-
Published:2017
Abstract
Bearings are usually provided where a specific spatial relationship (alignment) must be maintained between the parts or where a force is to be transmitted from one part to the other. This article introduces the general types and configuration of sliding bearings, bearing materials, and the practical aspects and solutions in the friction, lubrication, and wear mitigation of sliding bearings. The lubrication of bearings includes thick-film lubrication, thin-film lubrication, and boundary lubrication. The article concludes with a discussion on the effects of material elasticity on the lubrication of bearings.
Harish Hirani, Friction and Wear of Sliding Bearings, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 819–835, https://doi.org/10.31399/asm.hb.v18.a0006398
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.