Surface Texturing
-
Published:2017
Abstract
This article provides an overview of surface-texturing techniques. It describes the texturing parameters, namely, shape, depth, and width of the textured pattern, its aspect ratio (depth over width), texture area density, and orientation. The article explains the effect of these parameters on tribological behavior of textured surfaces. It provides information on various modeling approaches for surface texture. The article also discusses the beneficial effect of surface texturing.
Sign in
ASM members
Member Sign InBojan Podgornik, Surface Texturing, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 706–722, https://doi.org/10.31399/asm.hb.v18.a0006365
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.