Friction and Wear of Carbon-Containing Composites
-
Published:2017
Abstract
This article discusses the importance of friction and wear and the role of lubricants in composites. It highlights the progress and developments in using different forms of carbon allotropes in composites for improved friction and wear performance of materials. The article focuses on the widely used form known as carbon black (CB) and shows how to deal with friction and wear of polymers and composites when gamma irradiation is involved. It also discusses the role of graphite in composite materials, which is widely used as a dry lubricant. The article examines the tribology of carbon nanotubes (CNTs) as components...
Sign in
ASM members
Member Sign InDiana Berman, Witold Brostow, Haley E. Hagg Lobland, Jose M. Perez, Neelima Khare, Friction and Wear of Carbon-Containing Composites, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 550–558, https://doi.org/10.31399/asm.hb.v18.a0006367
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.