Laboratory Testing Methods for Solid Friction
-
Published:2017
Abstract
This article describes the numerous techniques used to measure friction. It provides a brief description of the historical development of friction testing. The article discusses the tests and equipment available for friction testing. It explains the procedural considerations that should be addressed to ensure that valid data are derived from a friction test. The article presents definitions of terms commonly used in tribology such as static friction, kinetic coefficient of friction, stick-slip behavior, and lubricated friction. It provides information on the precautions that must be taken to ensure valid test results. The article also describes how to report data...
Sign in
ASM members
Member Sign InK.G. Budinski, Laboratory Testing Methods for Solid Friction, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 44–55, https://doi.org/10.31399/asm.hb.v18.a0006361
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!